Mechanical Behaviour of Eutectic Superalloys

Published online by Cambridge University Press:  15 February 2011

M. McLean*
Affiliation:
Division of Materials Applications, National Physical Laboratory, Teddington, Middlesex TWIt OLW, UK
Get access

Extract

The mechanical properties of in-situ composites intended for use as gas turbine materials are reviewed. Particular emphasis is placed on the current understanding of strengthening and fracture mechanisms of these materials. The need to modify current methods of data representation, that have been developed for more conventional materials, in order to improve property extrapolation and design procedures are highlighted.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1982

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable