Abstract

Commercially pure Al was implanted with 300 keV Si+ and 200 keV Pb+ to doses of between l011 and 1017 ions/cm2. Changes in friction, wear, oxidation and hardness were investigated. Silicon increased the hardness and wear resistance of Al and significantly decreased friction and the oxidation of the implanted surface. These changes were observed to be almost proportional to the implanted dose. The implantation of Pb+ resulted in a linear increase in hardness and a decrease in surface oxidation with dose. Friction decreased and wear resistance increased but the changes were not dose dependent. The implantation of Si+ did not significantly alter the distribution of impurities, such as Fe and Cu within the Al matrix, but Pb+ resulted in a diffusion of Fe to the implanted surface. Formation of precipitates was observed and the improvements in the surface properties studied are considered to result from precipitation hardening, which involves the impediment of dislocation movement by the precipitates during plastic deformation of the implanted Al.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable