Hostname: page-component-7b7567c8c-z4zkx Total loading time: 0 Render date: 2026-11-18T04:17:45.186Z Has data issue: false hasContentIssue false

Oxygen-Induced Dynamic Embrittlement in Nickel-Base Superalloys

Published online by Cambridge University Press:  15 March 2011

C. J. McMahon Jr.
Affiliation:
Department of Materials Science and Engineering University of Pennsylania Philadelphia, PA 19104
W. M. Kane
Affiliation:
Department of Materials Science and Engineering University of Pennsylania Philadelphia, PA 19104
Get access

Abstract

The phenomenon of dynamic embrittlement involves the stress-induced diffusion of a surface- adsorbed embrittling element into grain boundaries, leading to time-dependent decohesion along these boundaries. Here, the state of our understanding of this generic type of brittle fracture is reviewed, with the focus on cracking of nickel-base superalloys caused by oxygen, including recent and new results on cracking in bicrystals, thermo-mechanical processing to reduce the susceptibility to dynamic embrittlement, and quench cracking.