Preparation and Sintering of Silica-Doped Zirconia by Colloidal Processing

Published online by Cambridge University Press:  10 February 2011

T. Uchikoshi
Affiliation:
National Research Institute for Metals, 1–2–1, Sengen, Tsukuba, Ibaraki 305, Japan
Y. Sakka
Affiliation:
National Research Institute for Metals, 1–2–1, Sengen, Tsukuba, Ibaraki 305, Japan
K. Ozawa
Affiliation:
National Research Institute for Metals, 1–2–1, Sengen, Tsukuba, Ibaraki 305, Japan
K. Hiraga
Affiliation:
National Research Institute for Metals, 1–2–1, Sengen, Tsukuba, Ibaraki 305, Japan
Get access

Abstract

Silica-doped (SiO2= 0–1.0 mass%) zirconia (3 mol% Y2O3-doped tetragonal ZrO2) compacts are prepared from hetero-coagulated and well-dispersed suspensions by colloidal processing. The suspensions are consolidated by a pressure filtration technique. The green density of the compacts consolidated from the well-dispersed suspensions is higher than that from the hetero-coagulated suspensions. The lower density of the latter compacts is improved by a subsequent cold isostatic pressing (CIP) at 400 MPa. The sinterability of the compacts at 1200 °C is greatly affected by the amount of doped silica. The densification and grain growth are hindered by silica doping above 0.3 wt% at 1200 °C. All the compacts are densificated to a relative density of above 99% by sintering at 1300 °C for 2 h.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1997

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable