Hostname: page-component-7b7567c8c-tnkh4 Total loading time: 0 Render date: 2026-11-17T16:39:18.528Z Has data issue: false hasContentIssue false

Rapidly Solidified NiAl and FeAl

Published online by Cambridge University Press:  21 February 2011

Darrell J. Gaydosh
Affiliation:
NASA Lewis Research Center, Cleveland, Ohio 44135
Martin A. Crimp
Affiliation:
Case Western Reserve University, Cleveland, Ohio 44106
Get access

Abstract

Melt spinning was used to produce rapidly solidified ribbons of the B2 intermetallics NiAl and FeAl. Both Fe-40Al and Fe-45A1 possessed some bend ductility in the as spun condition. The bend ductility of Fe-40Al, Fe-45Al, and equiatomic NiAl increased with subsequent heat treatment. Heat treatment at approximately 0.85 Tm resulted in significant grain growth in equiatomic FeAl and in all of the NiAl compositions. Low bend ductility in both FeAl and NiAl generally coincided with intergranular failure, while increased bend ductility was characterized by increasing amounts of transgranular cleavage fracture.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable