Published online by Cambridge University Press: 01 February 2011
This paper summarises our recent cyclic nanoindentation experiment studies on a range of materials including single crystal and nanocrystalline copper, single crystal aluminium and bulk metallic glasses with different glass transition temperatures. The unloading and reloading processes of the nanoindentation curves have been analysed. The reverse plasticity will be discussed in the context of plastic deformation mechanisms involved. The effect of loading rates on the mechanical properties of materials upon cyclic loading will also be discussed.