Hostname: page-component-7b7567c8c-8tzhz Total loading time: 0 Render date: 2026-11-19T14:26:22.790Z Has data issue: false hasContentIssue false

Silver Zeolites: Iodide Occlusion and conversion to Sodalite – a potential 129I waste form?

Published online by Cambridge University Press:  21 March 2011

Gareth P Sheppard
Affiliation:
School of Chemistry, University of Birmingham, Egbaston, Birmimingham, B15 2TT., UK
Joseph A Hriljac
Affiliation:
School of Chemistry, University of Birmingham, Egbaston, Birmimingham, B15 2TT., UK
Ewan R Maddrell
Affiliation:
Nexia Solutions, Sellafield, Seascale, Cumbria, CA20 1PG., UK
Neil C Hyatt
Affiliation:
Immobilisation Science Laboratory, Department of Engineering Materials, The University of Sheffield, Mappin Street, Sheffield, S1 3JD., UK
Get access

Abstract

Silver exchanged zeolites A, X and Y were used to occlude silver iodide (AgI) at 400°C. Heating to 900°C in a hot isostatic press caused decomposition of the zeolite materials and the formation of more dense phases. Silver zeolites A and X both formed sodalite, seen as a potential 129I waste form, while silver zeolite Y formed an x-ray amorphous phase containing AgI. Silver zeolite A produced the best potential waste form, a monolithic sodalite with negligible porosity.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable