Sintering Behavior of Ba2CaWO6-Doped-Tungsten

Published online by Cambridge University Press:  25 February 2011

J.A. Ruud
Affiliation:
General Electric Company, Corporate Research and Development Center, Schenectady, NY 12301
B.P. Bewlay
Affiliation:
General Electric Company, Corporate Research and Development Center, Schenectady, NY 12301
Get access

Abstract

The sintering behavior of Ba2CaWO6 co-sintered with W powder was investigated. Measurements of density and mass loss of sintered compacts showed that the Ba2CaWO6-doped-W had a lower density than undoped W and that there was little volatilization of Ba2CaWO6 at temperatures below 1750 °C. The activation energies for densification of Ba2CaWO6-doped-W and undoped W were both measured to be 389 kJ/mol, which indicates the same densification mechanism, grain boundary diffusion, operated for both materials. The reduced densification kinetics of the Ba2CaWO6-doped-W was probably due to increased coarsening in the early stages of sintering.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable