Hostname: page-component-7b7567c8c-fvjsw Total loading time: 0 Render date: 2026-11-16T08:52:55.652Z Has data issue: false hasContentIssue false

Sintering of AIN Powder Compacts

Published online by Cambridge University Press:  21 February 2011

M. Akaishi
Affiliation:
National Institute for Research in Inorganic Materials, Ibaraki, Japan
Y. Horie
Affiliation:
North Carolina State University, Raleigh, North Carolina
Get access

Abstract

Pure-AIN powder compacts have been fabricated by isostatic pressing and impact forming in the pressurs range of 1.5 ˜ 5.5 GPa. The density of these compacts was in the range of 70 ˜ 90% of the theoretical. The mean particle size was reduced from 20 μm to a few micron meters depending on compaction pressures. The density changes observed after sintering at temperatures above 1,600°C were independent of initial starting densities. A similar shrinkage was observed when residual strains were eliminated by annealing at 1,550°C for 30 min. Micro-structures of the sintered specimens showed a mixed region of either extensive grain growth or little growth.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable