Hostname: page-component-7b7567c8c-8p88z Total loading time: 0 Render date: 2026-11-19T10:36:21.322Z Has data issue: false hasContentIssue false

Solute Partitioning and Interfacial Segregation in TiAl-Based Alloys

Published online by Cambridge University Press:  10 February 2011

D. J. Larson
Affiliation:
Microscopy and Microanalysis Group, Metals and Ceramics Division, Oak Ridge National Laboratory, Oak Ridge, TN 3783 1-6376, larsondj @ornl.gov
M. K. Miller
Affiliation:
Microscopy and Microanalysis Group, Metals and Ceramics Division, Oak Ridge National Laboratory, Oak Ridge, TN 3783 1-6376, larsondj @ornl.gov
Get access

Abstract

Atom probe microscopy has been used to investigate elemental partitioning and segregation behavior in a TiAl-based alloy with a variety of alloying additions including Cr, Nb, W and B. These results indicate that in a stress-relieved state (2 h at 900°C) and a reheated state (2 h at 900°C, 2184 h at 800°C and 2 h at 1210°C) chromium, and to a lesser extent tungsten, is partitioned to the α2 phase. However, in an annealed state (2 h at 900°C and 720 h at 800°C), these elements are partitioned to the, γ phase. Segregation of chromium and tungsten to lamellar interfaces is observed in the stress-relieved material, but significant segregation was not observed in material subjected to the other heat treatments. A W- and B-enriched precipitate was observed in the reheated material and provides a possible explanation for the low tungsten concentrations measured in the matrix phases.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable