Stress evolution in integrated SrBi2Ta2O9 ferroelectric layers

Published online by Cambridge University Press:  01 February 2011

J. G. Lisoni
Affiliation:
IMEC, Silicon Process and Technology Devices Division, Leuven-Belgium
K. Wafer
Affiliation:
IMEC, Silicon Process and Technology Devices Division, Leuven-Belgium
J. A. Johnson
Affiliation:
IMEC, Silicon Process and Technology Devices Division, Leuven-Belgium
L. Goux
Affiliation:
IMEC, Silicon Process and Technology Devices Division, Leuven-Belgium
M. Schwitters
Affiliation:
IMEC, Silicon Process and Technology Devices Division, Leuven-Belgium
V. Paraschiv
Affiliation:
IMEC, Silicon Process and Technology Devices Division, Leuven-Belgium
D. Maes
Affiliation:
IMEC, Silicon Process and Technology Devices Division, Leuven-Belgium
L. Haspeslagh
Affiliation:
IMEC, Silicon Process and Technology Devices Division, Leuven-Belgium
C. Caputa
Affiliation:
STMicroelectronics, MPG Devt Center Catania, Catania-Italy
R. Zambrano
Affiliation:
STMicroelectronics, MPG Devt Center Catania, Catania-Italy
D. J. Wouters
Affiliation:
IMEC, Silicon Process and Technology Devices Division, Leuven-Belgium
Get access

Abstract

In our integration scheme, a “pseudo-3D” capacitor cell is used where the TiAlN\Ir\IrO2\Pt bottom electrode is patterned before SBT deposition. In order to understand how this system behaves mechanically, we have investigated the evolution of the stress of blanket Sr1-xBi2+yTa2O9 (x, y < 0.5) layers deposited on this pre-patterned bottom electrode stack. SBT was deposited by metal organic vapor deposition (MOCVD) between 405 °C and 440 °C. The stresses were monitored by the change in the radius of curvature of the wafer at the subsequent processing steps: deposition of electrodes and SBT, crystallization and recovering annealing, and after removal of Pt top electrode, SBT and bottom electrode layers by dry etching. The stress conditions observed for the different planar layers as a function of the SBT deposition temperature was correlated to the TiAlN lateral oxidation length observed in the etched structure after the SBT crystallization step.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2004

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable