Thermoelectric Power Studies on La2-xSrxNiO4-δ

Published online by Cambridge University Press:  15 February 2011

C.-J. Liu
Affiliation:
Department of Chemistry, The Johns Hopkins University, Baltimore, MD, 21218
M. G. Sánchez
Affiliation:
Department of Chemistry, The Johns Hopkins University, Baltimore, MD, 21218
D. O. Cowan
Affiliation:
Department of Chemistry, The Johns Hopkins University, Baltimore, MD, 21218
Get access

Abstract

Thermoelectric power (S) has been measured on La2-xSrxNiO4-δ. Both nonmetallic (0.5 < × < 1.0) and metallic materials (1.1 ≤ × ≤ 1. 5) have been investigated between 80 and 310 K. The sign of S changes from negative to positive between 150 and 220 K for both metallic and nonmetallic samples. The position at which the curve crosses from negative to positive depends upon the composition (x). For example, when × = 1.15 (metallic conductivity) S changes from negative to positive at about 220 K. However, if this sample is heated to 1000° C under argon, the material becomes nonmetallic and the sign of S remains positive between 80 and 310 K. These results may indicate that more than one type of carrier is involved. The absolute magnitude of S at 300 K decreases with × for 0.5 ≤ × ≤ 1.15 and then increases with × for 1.15 ≤ × ≤ 1.5. In the heavily doped material where S becomes more negative with increasing doping, the thermoelectric power strongly indicates that electrons and not holes are the majority carriers.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable