Toughening Effect and Oxidation Behavior of MoSi2 -ZrO2 Composites

Published online by Cambridge University Press:  26 February 2011

Karin Gong
Affiliation:
karin.gong@chalmers.se, Chalmers University of Technology, Materials and Manufacturing Technology, SE-412 96 Gothenburg,Sweden, Gothenburg, SE-412 96, Sweden, +46 31 7721251, +46 31 7721313
Yiming Yao
Affiliation:
yiming.yao@me.chalmers.se, Chalmers University of Technology, Materials and Manufacturing Technology, Gothenburg, SE-412 96, Sweden
Mats Sundberg
Affiliation:
mats.sundberg@kanthal.com, Kanthal AB, Hallstahammar, SE-734 27, Sweden
Xin-Hai Li
Affiliation:
xin-hai.li@siemens.com, Siemens Industrial Turbomachinery AB, Finspong, SE-612 82, Sweden
Erik Ström
Affiliation:
erik.strom@me.chalmers.se, Kanthal AB, Hallstahammar, SE-734 27, Sweden
Changhai Li
Affiliation:
changhai.li@me.chalmers.se, Chalmers University of Technology, Materials and Manufacturing Technology, Gothenburg, SE-412 96, Sweden
Get access

Abstract

Toughening effect of ZrO2-particles on MoSi2-based materials is one of the important toughening mechanism. In this work, the influence of particle size and volume percentage of unstabilized ZrO2-addition on toughening in MoSi2-matrix composites was studied. The measured data revealed that the fine particle size, < 1 ìm, with certain volume percentages around 20% have given more effective toughening results. The tested materials were prepared by two different sintering processes: pressure-less sintering (PLS) and PLS + Hipping sintering. The results on sintered density, RT-hardness and RT-toughness indicated that the PLS process could be a practical and economical method for producing MOSi2-ZrO2 composites in industry. Oxidation behavior of MoSi2-ZrO2 composites was also studied in the work. Clearly, the ZrO2-addition made the composites having a worse oxidation resistance than the monolithic MoSi2, which means that a low ZrO2-addition should be used in the composites, as far as an acceptable toughening effect was reached.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2007

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable