Wide-Gap Polysilane Produced by Plasma-Enhanced CVD at Cryogenic Temperatures

Published online by Cambridge University Press:  25 February 2011

S. Miyazaki
Affiliation:
Department of Electrical Engineering, Hiroshima University, Higashi-Hiroshima 724, Japan
H. Shin
Affiliation:
Department of Electrical Engineering, Hiroshima University, Higashi-Hiroshima 724, Japan
K. Okamoto
Affiliation:
Department of Electrical Engineering, Hiroshima University, Higashi-Hiroshima 724, Japan
M. Hirose
Affiliation:
Department of Electrical Engineering, Hiroshima University, Higashi-Hiroshima 724, Japan
Get access

Abstract

Polysilane thin films have been grown by the rf glow discharge decomposition of SiH4 at substrate temperatures ranging from -84 to -110°C. The infrared absorption spectra have shown that polysilane chains (SiH2)n are predominantly incorporated in the matrix together with SiH3 which terminates the chain. Also, the infrared absorption band at 2120∼2140 cm-1 and a distinct Raman peak at ∼430 cm-1indicates that fairly long chains (SiH2)n with n>11 are produced. Polysilane prepared at -110°C has an optical bandgap of about 3.1 eV and exhibits a visible luminescence around 2.75 eV at 100 K.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1992

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable