Hostname: page-component-7b7567c8c-z4zkx Total loading time: 0 Render date: 2026-11-17T17:48:02.051Z Has data issue: false hasContentIssue false

Aging Effect on the Microstructure of the Superalloy Inconel 939

Published online by Cambridge University Press:  01 February 2011

M. A. González
Affiliation:
Facultad de Ingeniería Mecánica y Eléctrica (FIME-UANL), Av. Universidad s/n. Ciudad Universitaria, C.P.66451 San Nicolás de los Garza, N.L., México
D. I. Martínez
Affiliation:
Facultad de Ingeniería Mecánica y Eléctrica (FIME-UANL), Av. Universidad s/n. Ciudad Universitaria, C.P.66451 San Nicolás de los Garza, N.L., México
A. Pérez
Affiliation:
Facultad de Ingeniería Mecánica y Eléctrica (FIME-UANL), Av. Universidad s/n. Ciudad Universitaria, C.P.66451 San Nicolás de los Garza, N.L., México
A. Garza
Affiliation:
Corporación Mexicana de Investigación en Materiales S.A. de C.V. (COMIMSA), Ciencia y Tecnología No.790, Saltillo 400, C.P. 25295 Saltillo Coah., Mexico. E-mail: mgonzalez@comimsa.com.mx
Get access

Abstract

In this work were evaluated the microestructural characteristics by Optical Microscopy (OM) and Scanning Electron Microscopy (SEM) of the intermetallic γ'(liquation, coarsening and decomposition) in the Inconel 939 alloy after 40000 hours and 850–900°C aging operation conditions. The alloy was vacuum conventional cast. The results show that the liquation phenomena take place in eutectics γ-γ' which are present mainly in the core of the dendritic arms and in the coarse films of carbides along the grain boundaries (GB), the γ' particles change their original morphology of ordered cuboids of 320nm to disordered and coarse cuboids of 1.2μm, carbides show a morphology change from the original dispersed particles into a coarse continuous films and particles Chinese script type, this affects adversely the mechanical properties such as creep. The results of this evaluation allow to determine the main microestructural damage mechanisms which experiment some components such as blades at high temperatures in industrial conditions.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable