AlN Films Deposited by LP-MOCVD Atomic Layer Deposition at Lower Temperatures Using DMEAA and Ammonia

Published online by Cambridge University Press:  21 February 2011

J.N. Kidder Jr.
Affiliation:
Department of Materials Science and Eng., University of Washington, Seattle, WA 98195
J. S. Kuo
Affiliation:
Department of Chemical Engineering, University of Washington, Seattle, WA 98195
T.P. Pearsall
Affiliation:
Department of Materials Science and Eng., University of Washington, Seattle, WA 98195
J.W. Rogers Jr.
Affiliation:
Department of Chemical Engineering, University of Washington, Seattle, WA 98195
Get access

Abstract

We have investigated the deposition of AlN thin films on Si(100), Al2O3(0001), and Al2O3(0112) substrates at lower temperatures (523–723 K) using a novel aluminum source, dimethylethylamine:alane (DMEAA), with ammonia as a nitrogen source in a low-pressure MOCVD atomic layer growth process. At reactor pressures of 25 and 50 Torr a four-step sequence of reactant flow steps separated by flush steps was cycled. We observed a tendency toward a self-limiting growth rate as the DMEAA step flow time was increased. The deposition uniformity was observed to be dependent on temperature and non-uniform deposition occurred at higher temperatures. The microstructure and crystalline orientation were examined using x-ray diffraction and crystalline A1N films were deposited at temperatures as low as 573 K. Crystallite size decreased with substrate temperature and at 523 K. amorphous films were deposited. At T > 650 K preferentially oriented crystalline films were deposited with orientations of Si(100)//AIN(0001), Al2O3(0001)//AIN(0001), Al2O3(0112)//AIN(11 20).

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)