Characterization Of Grown-In Defects In CZ-SI Crystals By Bright Field IR Laser Interferometer

Published online by Cambridge University Press:  15 February 2011

Katsuhiko Nakai
Affiliation:
Advanced Technology Research Laboratories, Nippon Steel Corporation, 3434 Shimata, Hikari, Yamaguchi 743, Japan
Masami Hasebe
Affiliation:
Advanced Technology Research Laboratories, Nippon Steel Corporation, 3434 Shimata, Hikari, Yamaguchi 743, Japan
Toshio Iwasaki
Affiliation:
Manufacturing Department, NSC Electron Corporation, 3434 Shimata, Hikari, Yamaguchi 743, Japan
Yasuo Tsumori
Affiliation:
Manufacturing Department, NSC Electron Corporation, 3434 Shimata, Hikari, Yamaguchi 743, Japan
Get access

Abstract

We have developed a quantitative measurement method for the number density, size and morphology of grown-in defects in czochralski-grown silicon (CZ-Si) crystals with a bright-field infrared-laser interferometer (known as Oxygen Precipitate Profiler; OPP). Using this method we investigated the effect of crystal cooling condition during crystal growth on the formation of grown-in defects by growth holding experiments. The relation between gate oxide integrity (GOI) and grown-in defects was studied. It was revealed that the grown-in defects have octahedral shape and degrade the GOI performance. We estimate the density as well as cumulative volume of the grown-in defects and discuss the formation mechanism of them.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1997

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable