Hostname: page-component-7b7567c8c-2n9c9 Total loading time: 0 Render date: 2026-11-17T02:27:00.163Z Has data issue: false hasContentIssue false

Compositional Effects on the Long-Term Durability of Nuclear Waste Glasses: A Statistical Approach

Published online by Cambridge University Press:  17 March 2011

Solange Ribet
Affiliation:
Vitreous State Laboratory, The Catholic University of America, Washington, D.C. 20064, USA, Isabellem@vsl.cua.edu
Isabelle S. Muller
Affiliation:
Vitreous State Laboratory, The Catholic University of America, Washington, D.C. 20064, USA
Ian L. Pegg
Affiliation:
Vitreous State Laboratory, The Catholic University of America, Washington, D.C. 20064, USA
Stéphane Gin
Affiliation:
CEAValRho DTCD/SECM/LCLT BP17171 30207 Bagnols-sur-Cèze, France
Pierre Frugier
Affiliation:
CEAValRho DTCD/SECM/LCLT BP17171 30207 Bagnols-sur-Cèze, France
Get access

Abstract

As a result of the development of a reference glass formulation for the immobilization of West-Valley nuclear waste, a large number of glass compositions have been tested under a variety of leaching conditions for extended durations. In this work, data from the standard PCT leaching procedure (deionized water, 90°C, S/V = 2000 m-1) are evaluated for a subset of 98 of these glasses, for which the alteration times extend up to fifteen years. Analysis of the leachate data over this extended period has led to a classification of the glass compositions according to their PCT behavior, as characterized by the boron release in solution, the decrease in the rate of alteration, or the occurrence of a resumption of alteration. Three types of behavior are associated with a normalized mass loss of boron after 100 days of around 1, 2, or 5 g m-2 respectively, and a ratio of the rate of alteration at 7 days to the rate at 1000 days of about 30. A fourth type is characterized by a much larger decrease between the rates at 7 and 1000 days with a ratio exceeding 120. Four further categories are associated with late-stage resumption of glass alteration. A statistical analysis of the data has been used to model the leachate data as a function of glass composition. The effects of seven major elements (Si, B, Al, Li, Na, K, Fe) on the long-term glass durability have been studied. As a result of this analysis, the different types of leaching behaviors can be predicted with a good reliability from the composition of the pristine glass.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable