Conductive Tungsten-Based Layers Synthesized by Ion Implantation Into 6H-Silicon Carbide

Published online by Cambridge University Press:  15 February 2011

H. Weishart
Affiliation:
Forschungszentrum Rossendorf e.V., Institut ffir Ionenstrahlphysik und Materialforschung, Postfach 510119, D-01314 Dresden, Germany
J. schöneich
Affiliation:
Forschungszentrum Rossendorf e.V., Institut ffir Ionenstrahlphysik und Materialforschung, Postfach 510119, D-01314 Dresden, Germany
M. Voelskow
Affiliation:
Forschungszentrum Rossendorf e.V., Institut ffir Ionenstrahlphysik und Materialforschung, Postfach 510119, D-01314 Dresden, Germany
W. Skorupa
Affiliation:
Forschungszentrum Rossendorf e.V., Institut ffir Ionenstrahlphysik und Materialforschung, Postfach 510119, D-01314 Dresden, Germany
Get access

Abstract

We studied high dose implantation of tungsten into 6H-silicon carbide in order to synthesize an electrically conductive layer. Implantation was performed at 200 keV with a dose of 1.2×1017 W+cm−2 at temperatures between 200°C and 400°C. The influence of implantation temperature on the distribution of W in SiC was investigated and compared to results obtained earlier from room temperature (RT) and 500°C implants. Rutherford backscattering spectrometry (RBS) was employed to study the structure and composition of the implanted layers. Implantation at temperatures between RT and 300°C did not influence the depth distribution of C, Si and W. The W depth profile shows a conventional Gaussian shape. Implanting at higher temperatures led to a more confined W rich layer in the SiC. This confinement is explained by Ostwald ripening which is enabled during implantation at temperatures above 300°C. The depth of the implantation induced damage decreases slightly with increasing implantation temperature, except for 400°C implantation. The amount of damage, however, is significantly reduced only for implantation at 500°C.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1997

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable