Hostname: page-component-7b7567c8c-tnkh4 Total loading time: 0 Render date: 2026-11-16T18:38:28.208Z Has data issue: false hasContentIssue false

Cross-Sectional TEM Study of Three-Dimensional MOS Devices

Published online by Cambridge University Press:  28 February 2011

Kyung-Ho Park
Affiliation:
Fujitsu Ltd., Advanced Technology Division, 1015 Kamikodanaka, Nakahara-ku, Kawasaki, 211, JAPAN
T. Sasaki
Affiliation:
Fujitsu Ltd., Advanced Technology Division, 1015 Kamikodanaka, Nakahara-ku, Kawasaki, 211, JAPAN
T. Iwai
Affiliation:
Fujitsu Ltd., Advanced Technology Division, 1015 Kamikodanaka, Nakahara-ku, Kawasaki, 211, JAPAN
M. Hasegawa
Affiliation:
Fujitsu Ltd., Advanced Technology Division, 1015 Kamikodanaka, Nakahara-ku, Kawasaki, 211, JAPAN
N. Sasaki
Affiliation:
Fujitsu Ltd., Advanced Technology Division, 1015 Kamikodanaka, Nakahara-ku, Kawasaki, 211, JAPAN
Get access

Abstract

This paper describes cross-sectional transmission electron microscopy (TEM) observation on finished 3-D MOS devices, fabricated with a laser-recrystallized SOI. The laser-recrystallized SOI contained crystal defects such as micro-twinning, grain boundaries and dislocations. It is also clearly shown that the interface roughness between the gate oxide and SOI is as much as 20 nm height, in where the interface is very smooth between the gate oxide and bulk silicon.