Hostname: page-component-7b7567c8c-wxvwp Total loading time: 0 Render date: 2026-11-16T06:27:13.960Z Has data issue: false hasContentIssue false

Defect Tails in GE Implanted Si Probed by Slow Positrons and Ion Channeling

Published online by Cambridge University Press:  10 February 2011

A P Knights
Affiliation:
School of Electronic Engineering, Information Technology and Mathematics, University of Surrey, Guildford GU2 5XH, United Kingdom. a.knights@ee.surrey.ac.uk
A Nejim
Affiliation:
School of Electronic Engineering, Information Technology and Mathematics, University of Surrey, Guildford GU2 5XH, United Kingdom. a.knights@ee.surrey.ac.uk
N P Barradas
Affiliation:
School of Electronic Engineering, Information Technology and Mathematics, University of Surrey, Guildford GU2 5XH, United Kingdom. a.knights@ee.surrey.ac.uk
R Gwilliam
Affiliation:
School of Electronic Engineering, Information Technology and Mathematics, University of Surrey, Guildford GU2 5XH, United Kingdom. a.knights@ee.surrey.ac.uk
P G Coleman
Affiliation:
School of Physics, University of East Anglia, Norwich, NR4 7TJ, United Kingdom.
F Malik
Affiliation:
School of Physics, University of East Anglia, Norwich, NR4 7TJ, United Kingdom.
H Kherandish
Affiliation:
MATS UK, Innovation House, Daten Park, Warrington, WA3 6UT, United Kingdom.
S Romani
Affiliation:
MATS UK, Innovation House, Daten Park, Warrington, WA3 6UT, United Kingdom.
Get access

Abstract

Positron annihilation spectroscopy has been used to profile the distribution of defects following implantation of 120keV Ge+ into (100) Si in the dose range l x 1010 - lx104 cm−2 . The openvolume defect profiles can be adequately fitted assuming a simple rectangular block distribution extending to 350nm. Using anodic oxidation and etching, a procedure is described which allows details of the defect tails beyond the range of the implanted ion, usually inaccessible to positron -2 annihilation measurements, to be determined. For a time averaged dose-rate (Jr) of 0.02μA cm−2 and incident angle of 7°, open-volume defects are found to exist at concentrations exceeding 1016cm−3 at depths upto 600nm whereas the peak of the depth distribution of the implanted ions (Rp) is 76nm, measured using SIMS. When the time-average dose-rate is increased by a factor of 10, defects persist at concentrations in excess of 1017cm−3 beyond lμm and the Rp increases to 101nm. The open-volume defect profiles are compared to those deduced from Rutherford backscattering-channeling using the fitting routine DICADA.