Hostname: page-component-7b7567c8c-z4zkx Total loading time: 0 Render date: 2026-11-17T16:31:30.621Z Has data issue: false hasContentIssue false

Evolution of Nanostructure of FeNi(Ti/Cr)N Alloys During Phase Cycling

Published online by Cambridge University Press:  21 March 2011

N. G. Chechenin
Affiliation:
Materials Science Center, University of Groningen, Nijenborgh 4, NL 9747 AG Groningen, The Netherlands
P. M. Bronsveld
Affiliation:
Materials Science Center, University of Groningen, Nijenborgh 4, NL 9747 AG Groningen, The Netherlands
A. R. Chezan
Affiliation:
Materials Science Center, University of Groningen, Nijenborgh 4, NL 9747 AG Groningen, The Netherlands
C. B. Craus
Affiliation:
Materials Science Center, University of Groningen, Nijenborgh 4, NL 9747 AG Groningen, The Netherlands
D. O. Boerma
Affiliation:
Materials Science Center, University of Groningen, Nijenborgh 4, NL 9747 AG Groningen, The Netherlands
J. Th.M. de Hosson
Affiliation:
Materials Science Center, University of Groningen, Nijenborgh 4, NL 9747 AG Groningen, The Netherlands
L. Niesen
Affiliation:
Materials Science Center, University of Groningen, Nijenborgh 4, NL 9747 AG Groningen, The Netherlands
Get access

Abstract

A possibility to manipulate the microstructure of cold rolled (down to less than 1% of the initial thickness) Fe94Ni4Ti2 and Fe93Ni4 Cr3 foils via inter-phase cycling by nitriding and de-nitriding is investigated. The grains in the as-rolled material had a dominating (001)[110] texture and contained a complicated internal nanostructure due to a dislocation network. The interphase cycling α↔γ'-Fe4N and α↔ε-FexN (x∼3) was investigated as a tool to change or destroy the texture. We observed that the α↔γ'-Fe4N phase transformations weaken but do not erase the texture. A stronger reduction of the texture was obtained in the α↔ε-cycling, where grains with a new orientation appear in XRD scans. During the α↔γ' phase transformation a lamella structure is formed which is coarsening with the number of cycles. It was found that the rates of the α↔γ' and α↔ε interphase transitions were slowing down with the number of cycles. The observation is explained by an increase of kinetic barriers while removing/transforming the rolling-induced defects during the cycling.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable