Hostname: page-component-7b7567c8c-tnkh4 Total loading time: 0 Render date: 2026-11-17T13:43:46.086Z Has data issue: false hasContentIssue false

Experimental and Computational Studies of Ion-Solid Interactions in Silicon Carbide

Published online by Cambridge University Press:  01 February 2011

William J. Weber
Affiliation:
Fundamental Science Directorate, Pacific Northwest National Laboratory, Richland, WA 99352, U.S.A.
Fei Gao
Affiliation:
Fundamental Science Directorate, Pacific Northwest National Laboratory, Richland, WA 99352, U.S.A.
Ram Devanathan
Affiliation:
Fundamental Science Directorate, Pacific Northwest National Laboratory, Richland, WA 99352, U.S.A.
Weilin Jiang
Affiliation:
Fundamental Science Directorate, Pacific Northwest National Laboratory, Richland, WA 99352, U.S.A.
Yanwen Zhang
Affiliation:
Fundamental Science Directorate, Pacific Northwest National Laboratory, Richland, WA 99352, U.S.A.
Get access

Abstract

Experimental and computational results on ion-beam-induced defect production, damage accumulation, and thermal recovery in SiC are reviewed. The accumulation and recovery of disorder on the Si and C sublattices have been determined experimentally by ion-channeling methods. Atomic-level simulations are used to determine defect production, cascade-overlap effects, and defect migration energies. Energetic Si and C collision cascades, with energies up to 50 keV, primarily produce single interstitials, mono-vacancies, antisite defects, and small defect clusters. Overlapping of Si and C cascades results in the interaction of defects and clusters that stimulates cluster growth and produces long-range structural disorder. For energetic Au cascades, nanoscale amorphous clusters are produced directly within about 25% of the Au cascades, along with point defects and smaller clusters. The disordering behavior and the changes in volume and elastic modulus obtained experimentally and from molecular dynamics simulations are in good agreement, thus providing atomic-level interpretation of experimentally observed features. Simulations of close-pair production and recombination in SiC indicate that the activation energies for recombination of most close pairs range from 0.24 to 0.38 eV. Multiaxial channeling measurements indicate annealing below 300 K results in relaxation of some interstitials to lower-energy configurations. Long-range migration energies for interstitials and vacancies have likewise been determined by computational methods.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable