Hostname: page-component-7b7567c8c-tnkh4 Total loading time: 0 Render date: 2026-11-17T12:18:48.511Z Has data issue: false hasContentIssue false

Fracture Toughness of Diamond Measured by Vickers Indenter Reloading Technique

Published online by Cambridge University Press:  15 February 2011

Sergey N. Dub*
Affiliation:
Institute for Superhard Materials of the Ukrainian National Academy of Sciences, 2 Avtozavodskaya Str., Kiev, 254074, Ukraine
Get access

Abstract

The crack initiation sequence during Vickers indenter penetration into the (100) plane of diamond was observed. It was revealed that for <110> orientation, two median cracks are initiated during the loading half of the cycle. In unloading, the median cracks grow toward the surface and turn into half-penny cracks. It was proposed to use half-penny cracks as initials and evaluate fracture toughness in second loading from a crack-starting load for these cracks. The length of initial half-penny cracks was measured after first loading cycle from opposite side of the sample. Test results obtained by the reloading technique agree well with the data on conventional fracture toughness determination by indentation from the length of cracks after unloading.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable