High Temperature Electrical Conductivity Of Solution-Cast Bbl Flims.

Published online by Cambridge University Press:  16 February 2011

Ashwini K. Agrawal
Affiliation:
Systran Corporation, 4126 Linden avenue, Dayton, OH 45432
Chyi-Shan Wang
Affiliation:
University of Dayton Research Institute, 300 College Park Drive, Dayton, OH 45469
Hyun H. Song
Affiliation:
University of Dayton Research Institute, 300 College Park Drive, Dayton, OH 45469
Get access

Abstract

Thin films (18 μ thickness) of ladder polymer poly[(7-oxo-7H,10H-benz (d,e) imidazo (4′,5′:5,6) -benzimidazo (2,l-a) isoquinoline-3,4:10,ll-tetrayl)-10-carbonyl} (BBL), which were cast from an isotropie methanesulfonic acid solution of BBL, were characterized for electrical conductivity in the temperature range of 25–480 °C. The electrical conductivity was Measured in situ while the films were heated at a rate of 2 °C/Minute under vacuum. The in-plane conductivity of BBL films increased rapidly from below 10−10 S/cm at the room temperature to 5 × 10-3 S/cm at 280 °C and then increased slowly to a peak value of 5 × 10-2 S/cm at about 460 °C. The out-of-plane conductivity of the films was comparable to their in plane conductivity at temperatures below 270 °C, however, was lower by a factor of 10 than in-plane conductivity at temperatures above 270 °C. This anisotropy in conductivity of BBL films is discussed with respect to the film morphology determined by wide angle x-ray scattering studies.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable