Hostname: page-component-7b7567c8c-tnkh4 Total loading time: 0 Render date: 2026-11-17T06:43:59.150Z Has data issue: false hasContentIssue false

High Temperature Mechanical Behavior of SiCf/Ti–Al Composites

Published online by Cambridge University Press:  01 January 1992

H.Y. Chou
Affiliation:
Materials R&D Center, CSIST, P.O. Box 90008–8, Lungtan, Taiwan, R.O.C.
S.C. Yang
Affiliation:
Materials R&D Center, CSIST, P.O. Box 90008–8, Lungtan, Taiwan, R.O.C.
K.L. Wang
Affiliation:
Materials R&D Center, CSIST, P.O. Box 90008–8, Lungtan, Taiwan, R.O.C.
C.I. Chen
Affiliation:
Materials R&D Center, CSIST, P.O. Box 90008–8, Lungtan, Taiwan, R.O.C.
S.E. Hsu
Affiliation:
Materials R&D Center, CSIST, P.O. Box 90008–8, Lungtan, Taiwan, R.O.C.
Get access

Abstract

Titanium aluminide was reinforced by AVCO SCS–6 continuous SiC fibers in unidirectional or 0°/+45°/–45° direction to make SiCf/Ti–A1 composites through hot-pressing of Ti and A1 powder mixture. The toughness of the composites is greatly improved at room temperature. The typical tensile elongation is over 0.8%. The room temperature strength of the composite can be sustained up to about 700°C. The processes developed in this study have two merits: (1) Ti and A1 powders instead of Ti–A1 powder can be directly used as raw materials, and (2) the mechanical properties of composites can be tailored in a similar fashion as those of conventional composites.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable