High-Temperature Strength of Ir-Based Refractory Superalloys

Published online by Cambridge University Press:  21 March 2011

Yoko Yamabe-Mitarai*
Affiliation:
High-Temperature Materials 21st Project (HTM21), National Research Institute for Metals, 1–2–1 Sengen, Tsukuba, Ibaraki 305–0047, Japan
Get access

Abstract

Ir-based refractory superalloys with an fcc and L12 two-phase structure similar to that in Ni-based superalloys but with considerably higher melting temperatures are proposed. First, the microstructure and strength are shown for several kinds of binary alloys. Then, the effect that the third element and the combination of Ni-Al with an fcc and L12 two-phase structure in binary alloys had on the lattice misfit, microstructure, and strength was investigated. The precipitation-hardening effect in Ir-based alloys was investigated and discussed in terms of precipitate morphology and lattice misfit. The creep properties of Ir-based alloys were also investigated.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2001

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable