Identification of Pressure-Induced Phase Transformations Using Nanoindentation

Published online by Cambridge University Press:  17 March 2011

Vladislav Domnich
Affiliation:
Department of Mechanical Engineering, University of Illinois at Chicago, 842 West Taylor Street, Chicago, IL 60607, USA
Yury Gogotsi
Affiliation:
Department of Materials Engineering, Drexel University, 3141 Chestnut Street, Philadelphia, PA 19104, USA
Michael Trenary
Affiliation:
Department of Chemistry, University of Illinois at Chicago, 845 West Taylor Street, Chicago, IL 60607, USA
Get access

Abstract

A combination of depth-sensing indentation and Raman microspectroscopy has been used for the identification of pressure-induced phase transformations in silicon, germanium, boron carbide and partially stabilized zirconia single crystals. Phase transformations during nanoindentation may be revealed through deviations in the shape of the load-displacement curves from that of a perfect elastoplastic material. Such deviations are often more readily identified if the nanoindentation data are presented as average contact pressure vs. contact depth curves, allowing assessment of the corresponding transformation pressures.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable