The Impact of Increased Waste Loading on Vitrified HLW Quality and Durability

Published online by Cambridge University Press:  15 February 2011

Nick R Gribble
Affiliation:
National Nuclear Laboratory, Sellafield, Seascale, Cumbria, CA20 1PG, Cumbria
Rick Short
Affiliation:
National Nuclear Laboratory, Sellafield, Seascale, Cumbria, CA20 1PG, Cumbria
Edward Turner
Affiliation:
National Nuclear Laboratory, Sellafield, Seascale, Cumbria, CA20 1PG, Cumbria
Andrew D Riley
Affiliation:
Sellafield Ltd, Sellafield, Seascale, Cumbria, CA20 1PG, Cumbria
Get access

Abstract

The Sellafield Waste Vitrification Plant (WVP) immobilises highly active liquid waste (HAL) arising from the reprocessing of spent nuclear fuel in the UK. In order to optimise WVP operations a full scale working replica of a WVP processing line, the Vitrification Test Rig (VTR), was constructed to processes non-active HAL simulants. Recently the VTR has been used to determine an operational envelope for the vitrification of HAL from Magnox reprocessing at a waste oxide incorporation rate in glass of up to 35wt% (compared to a “standard” incorporation rate of 25wt%). This paper discusses the differences in operating conditions necessary to achieve acceptable waste throughput at the increased incorporation rate. The chemical durability of the resulting vitrified product is also discussed, along with the formation of secondary phases, and a comparison is drawn between 35wt% incorporation glasses and products made at the standard 25wt% incorporation.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2009

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable