Hostname: page-component-7b7567c8c-8tzhz Total loading time: 0 Render date: 2026-11-19T17:36:02.492Z Has data issue: false hasContentIssue false

Indentation Modulus and Yield Point of Au (111), (001), and (110)

Published online by Cambridge University Press:  10 February 2011

J. D. Kiely
Affiliation:
Surface and Interface Sciences Department, MS 1413 Sandia National Laboratories, Albuquerque, NM 87185-1413
J. E. Houston
Affiliation:
Surface and Interface Sciences Department, MS 1413 Sandia National Laboratories, Albuquerque, NM 87185-1413
Get access

Abstract

Nanoscale indentation experiments were performed on Au using the Interfacial Force Microscope (IFM) in an indentation mode. The indentation modulus and yield point were measured for three orientations of the Au surface: (111), (110), and (001). The indentation modulus for the (111) surface was found to be 36% greater than for the (001) surface and only 3% higher than the (110) surface. Additionally, the yield point was found to vary between orientations, but the shear stress resolved on {111} slip planes beneath the indenter on the axis of symmetry was found to be approximately 1.8 GPa for yield points of all three orientations.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable