Ion-Beam-Modified Interfacial Growth of Tungsten Disilicide

Published online by Cambridge University Press:  26 February 2011

E. Ma
Affiliation:
California Institute of Technology, Pasadena, CA 91125
N. S. Alvi
Affiliation:
Delco Electronics Corporation, 700 East Firmin Street, Kokomo IN 46902
A. H. Hamdi
Affiliation:
Electronics Department, General Motors Research Laboratories, Warren, MI 48090-9055
M-A. Nicolet
Affiliation:
California Institute of Technology, Pasadena, CA 91125
Get access

Abstract

Preimplantation of phosphorous is used in this work to promote the lateral uniformity of the interfacial WSi2 layer that grows upon subsequent thermal annealing of a thin W film sputter-deposited on a monocrystalline Si substrate. A phosphorous dose of 7.5x1015 P/cm2 yields an intermixed layer at the interface and the formation of the low-temperature hexagonal WSi2 phase. Subseqent vacuum furnace annealing at temperatures from 630°C to 715°C leads to a laterally uniform growth of tetragonal WSi2. The kinetics concur with those of previous reports for diffusion-limited growth of WSi2. All the available data fit well with a common growth law of x2 =kt, in which x is the thickness of the silicide layer, t is the annealing duration and k is the growth constant. The growth constant is given by k=1.5x104(cm2/s)exp(Ea/kBT), where the activation energy Ea=3.5±0.3 eV. Possible factors responsible for the beneficial effect of ion mixing on the interfacial silicide growth is discussed.