Hostname: page-component-7b7567c8c-tnkh4 Total loading time: 0 Render date: 2026-11-17T22:31:19.590Z Has data issue: false hasContentIssue false

Mechanisms of Stress Corrosion Cracking in Si: A Hybrid Quantum-Mechanical/Molecular-Dynamics Simulation

Published online by Cambridge University Press:  11 February 2011

Rachid Belkada
Affiliation:
Japan Science and Technology Corporation, Kawaguchi 332–0012, JapanDepartment of Applied Sciences, Yamaguchi University, Ube 755–8611, Japan
Shuji Ogata
Affiliation:
Department of Applied Sciences, Yamaguchi University, Ube 755–8611, Japan
Fuyuki Shimojo
Affiliation:
Departemnet of Physics, Kumamoto University, Kumamoto 860–8555, Japan
Aiichiro Nakano
Affiliation:
CCLMS, Louisiana State University, Baton Rouge, LA70803–4001, U.S.ADepartement of Computer Science, University of Southern California, Los Angeles, CA90089–0242, U.S.A.
Priya Vashishta
Affiliation:
CCLMS, Louisiana State University, Baton Rouge, LA70803–4001, U.S.ADepartement of Computer Science, University of Southern California, Los Angeles, CA90089–0242, U.S.A.
Rajiv K. Kalia
Affiliation:
CCLMS, Louisiana State University, Baton Rouge, LA70803–4001, U.S.ADepartement of Computer Science, University of Southern California, Los Angeles, CA90089–0242, U.S.A.
Get access

Abstract

We investigate mechanisms of stress corrosion cracking in Si using a hybrid quantum-mechanical/molecular-dynamics simulation code developed recently for parallel computers. We perform the simulation for a cracked Si-model under tension (mode-I opening) with three H2O molecules around the crack front to investigate possible effects of both saturation of dangling bonds of Si with hydrogen atoms and environment molecules on the fracture initiation. Our results demonstrate existence of a path for an H2O molecule to react with Si-Si bonds at the crack front in contrast to a previous theoretical study based on the molecular orbital theory [W. Wong-Ng et al., Comp. Mater. Sci. 6, 63 (1996)].

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable