Hostname: page-component-7b7567c8c-tnkh4 Total loading time: 0 Render date: 2026-11-16T04:47:47.852Z Has data issue: false hasContentIssue false

A Method for Extracting Quantitative Data During in-situ TEM Nanoindentation

Published online by Cambridge University Press:  21 March 2011

A.M. Minor
Affiliation:
Department of Materials Science & Engineering, University of California, Berkeley, CA
E.T. Lilleodden
Affiliation:
Materials Science Division, Lawrence Berkeley National Laboratory, Berkeley, CA
E.A. Stach
Affiliation:
National Center for Electron Microscopy, Lawrence Berkeley National Laboratory, Berkeley, CA.
J.W. Morris
Affiliation:
Department of Materials Science & Engineering, University of California, Berkeley, CAMaterials Science Division, Lawrence Berkeley National Laboratory, Berkeley, CA
Get access

Abstract

The development of a novel transmission electron microscope holder has made real time observations of nanoindentation possible. Using a piezo-ceramic loading mechanism, a diamond indenter is pushed into the surface of a sample, while the electron beam images the deforming sample in cross section. In this paper, we present the method for calibrating the force-displacement-voltage relation and load-frame compliance associated with this instrument. This allows quantitative force-displacement measurements to be obtained, in the manner of traditional indentation experiments. As an example of the utility of this technique, we present observations of the indentation behavior of an Al thin film on silicon, which have been previously shown [1]. Indentation into a coarse grain shows a displacement excursion corresponding to the nucleation of dislocations, and is compared to force-displacement responses measured with instrumented indentation techniques.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable