Hostname: page-component-7b7567c8c-tnkh4 Total loading time: 0 Render date: 2026-11-17T14:56:22.534Z Has data issue: false hasContentIssue false

Nanoindentation Behavior of Gold Single Crystals

Published online by Cambridge University Press:  01 February 2011

Martha M. McCann
Affiliation:
Virginia Tech, Department of Materials Science and Engineering, Blacksburg, VA 24061
Sean G. Corcoran
Affiliation:
Virginia Tech, Department of Materials Science and Engineering, Blacksburg, VA 24061
Get access

Abstract

Nanoindentation is an increasingly used tool to investigate the mechanical properties of very small volumes of material. It is usually a very consistent measure of the elastic response of material and plastic response to point contact loading. Nanoindentation experiments on gold single crystals display tremendous variation in the residual deformation. The depth of penetration, which is vital in hardness determination, can differ by as much as 100%. This large variability of the load-depth data is usually explained by surface differences such as crystal orientation, oxide thic kness, presence of multiple solid phases, or contamination layers. None of these reasons apply to the variation observed in the gold system. The onset of plastic deformation is observed at a stress level on the order of the theoretical yield strength. The difference in depth of penetration is independent of this elastic -plastic transition. This paper reports on attempts to correlate the depth of penetration to surface feature size and surface preparation procedures.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable