Nanoindentation on Contamination-Free gold Films Using the Atomic Force Microscope

Published online by Cambridge University Press:  21 February 2011

D. M. Schaefer
Affiliation:
Purdue University, Department of Physics, W. Lafayette IN 47907
R. Reifenberger
Affiliation:
Purdue University, Department of Physics, W. Lafayette IN 47907
Get access

Abstract

Nanoindentation experiments on high quality Au films were performed in vacuum using an atomic force microscope. In these experiments, elastic behavior was observed until loading forces greater than ∼ 20 nN were applied. For loads larger than this, systematic changes in the jump-to-contact, loading/unloading and lift-off regions of the data occur. These observations are consistent with a transition from elastic to inelastic behavior during indentation.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable