Hostname: page-component-7b7567c8c-7pwfn Total loading time: 0 Render date: 2026-11-16T08:40:30.598Z Has data issue: false hasContentIssue false

New Pt-based Superalloy System Designed from First Principles

Published online by Cambridge University Press:  21 September 2018

Vsevolod I. Razumovskiy
Affiliation:
Applied Materials Physics, Department of Materials Science and Engineering, Royal Institute of Technology, SE-100 44 Stockholm, SwedenDepartment of Theoretical Physics, Moscow Institute of Steel and Alloys, 119049 Moscow, Russia
Eyvaz I. Isaev
Affiliation:
Department of Theoretical Physics, Moscow Institute of Steel and Alloys, 119049 Moscow, RussiaCondensed Matter Theory Group, Department of Physics, Uppsala University, Box 530, SE- 751 21 Uppsala, SwedenDepartment of Physics, Chemistry and Biology (IFM), Linköping University, SE-581 83 Linköping, Sweden
Andrei V. Ruban
Affiliation:
Applied Materials Physics, Department of Materials Science and Engineering, Royal Institute of Technology, SE-100 44 Stockholm, Sweden
Pavel A. Korzhavyi
Affiliation:
Applied Materials Physics, Department of Materials Science and Engineering, Royal Institute of Technology, SE-100 44 Stockholm, Sweden
Get access

Abstract

Pt-Sc alloys with the γ-γ′ microstructure are proposed as a basis for a new generation of Pt-based superalloys for ultrahigh-temperature applications. This alloy system was identified on the basis of first-principles calculations. Here we discuss the prospects of the Pt-Sc alloy system on the basis of calculated elastic properties, phonon spectra, and defect formation energies.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)