Platinum Group Metals Base Refractory Superalloys

Published online by Cambridge University Press:  15 February 2011

Y. Yamabe-Mitarai
Affiliation:
National Research Institute for Metals, 1–2–1 Sengen, Tsukuba, Ibaraki, 305, Japan, yamabe@tamamori.nrim.go.jp
Y. Koizumi
Affiliation:
National Research Institute for Metals, 1–2–1 Sengen, Tsukuba, Ibaraki, 305, Japan, yamabe@tamamori.nrim.go.jp
H. Murakami
Affiliation:
National Research Institute for Metals, 1–2–1 Sengen, Tsukuba, Ibaraki, 305, Japan, yamabe@tamamori.nrim.go.jp
Y. Ro
Affiliation:
National Research Institute for Metals, 1–2–1 Sengen, Tsukuba, Ibaraki, 305, Japan, yamabe@tamamori.nrim.go.jp
T. Maruko
Affiliation:
National Research Institute for Metals, 1–2–1 Sengen, Tsukuba, Ibaraki, 305, Japan, yamabe@tamamori.nrim.go.jp
H. Harada
Affiliation:
National Research Institute for Metals, 1–2–1 Sengen, Tsukuba, Ibaraki, 305, Japan, yamabe@tamamori.nrim.go.jp
Get access

Abstract

Ir- and Rh-base refractory superalloys with an fee and Lb two phase structure similar to Ni-base superalloys, yet with considerably higher melting temperatures have been proposed. Fee and Ll2 two phases were observed in these alloys by transmission electron microscopy and X-ray powder diffractometry. The compression tests of these alloys showed that the strengths of several alloys were about 200 MPa at 1800 °C and these alloys have potential to become ultra-high temperature materials for use in power engineering field.