Hostname: page-component-7b7567c8c-wxvwp Total loading time: 0 Render date: 2026-11-19T00:59:54.004Z Has data issue: false hasContentIssue false

Preparation and Characterization of LiCoO2 and LiMg0.05Co0.95O2 Thin Films on Porous Ni/NiO Cathodes for MCFC by Complex Sol-Gel Process (CSGP)

Published online by Cambridge University Press:  10 February 2011

W. Lada
Affiliation:
Institute of Nuclear Chemistry and Technology, 03-195 Warsaw, Poland, adept@orange.ichtj.waw.pl
A. Deptula
Affiliation:
Institute of Nuclear Chemistry and Technology, 03-195 Warsaw, Poland, adept@orange.ichtj.waw.pl
B. Sartowska
Affiliation:
Institute of Nuclear Chemistry and Technology, 03-195 Warsaw, Poland, adept@orange.ichtj.waw.pl
T. Olczak
Affiliation:
Institute of Nuclear Chemistry and Technology, 03-195 Warsaw, Poland, adept@orange.ichtj.waw.pl
A.G. Cimielewski
Affiliation:
Institute of Nuclear Chemistry and Technology, 03-195 Warsaw, Poland, adept@orange.ichtj.waw.pl
M. Carewska
Affiliation:
ENEA, TEA-CCAT, Casaccia Casaccia, AD 00100 Roma, Italy
S. Scaccia
Affiliation:
ENEA, TEA-CCAT, Casaccia Casaccia, AD 00100 Roma, Italy
E. Simonetti
Affiliation:
ENEA, TEA-CCAT, Casaccia Casaccia, AD 00100 Roma, Italy
L. Giorgi
Affiliation:
ENEA, TEA-CCAT, Casaccia Casaccia, AD 00100 Roma, Italy
A. Moreno
Affiliation:
ENEA, TEA-CCAT, Casaccia Casaccia, AD 00100 Roma, Italy, moreno@casaccia.enea.it
Get access

Abstract

The major disadvantage of Ni/NiO cathodes for a Molten Carbonate Fuel Cells (MCFC) application is dissolution of NiO in K/Li electrolyte that significantly decreases the cell lifetime. Thin films of LiCoO2 or LiMg0.05Co0.9502 were prepared on a cathode body in order to protect them against dissolution. For preparation of starting sols the Complex Sol-Gel Process (CSGP) has been applied. These sols have been prepared by adding of LiOH to aq. acetates solution of Co 2+(Mg2+) with ascorbic acid and then by alkalizing them with aqueous ammonia to pH=8. The cathode plates of various dimensions (to several hundreds cm2) have been dipped in these sols and withdrawn at rate a 1.7 cm/s. Commercially sintered Ni plates were always initially oxidized by heating at various temperatures. Their microstructure and mechanical properties as a function of temperature were observed. Heat treatment should be carried out under the dead load of the ceramic plates in order to avoid their waving. The best non-folded plates were obtained by treating them for lh at 550°C. The covered substrates were calcined for lh at 650°C, using low heating ratel°C/min. The presence of LiCoO2 in a deposited coating has been proved by EDS patterns. The resultant film thicknesses were measured by scanning electron microscopy (SEM) on the fractured cross-sections; they ranged from 0.5 to 2νm and depended on sol concentration and viscosity. A 350 hundred hours test in molten carbonates, proved that the cathode bodies covered with LiCoO2 are completely prevented from dissolution of Ni in a molten K/Li electrolyte. Dissolution of LiCoO2 coating was not observed as well. After treatment in a molten electrolyte SEM observations did not show any changes in microstructures and morphology of the covered cathodes.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable