Hostname: page-component-7b7567c8c-8tzhz Total loading time: 0 Render date: 2026-11-19T13:05:12.893Z Has data issue: false hasContentIssue false

Preparation of Optoelectronic Devices Based on AlN/AlGaN Superlattices

Published online by Cambridge University Press:  11 February 2011

M. Holtz
Affiliation:
Department of Physics, Texas Tech University, Lubbock, Texas 79409Nano Tech Center, Texas Tech University, Lubbock, Texas 79409
G. Kipshidze
Affiliation:
Department of Electrical Engineering, Texas Tech University, Lubbock, Texas 79409
A. Chandolu
Affiliation:
Department of Electrical Engineering, Texas Tech University, Lubbock, Texas 79409
J. Yun
Affiliation:
Department of Electrical Engineering, Texas Tech University, Lubbock, Texas 79409
B. Borisov
Affiliation:
Department of Electrical Engineering, Texas Tech University, Lubbock, Texas 79409
V. Kuryatkov
Affiliation:
Department of Electrical Engineering, Texas Tech University, Lubbock, Texas 79409
K. Zhu
Affiliation:
Department of Electrical Engineering, Texas Tech University, Lubbock, Texas 79409
S. N. G. Chu
Affiliation:
Agere Systems, Murray Hill, NJ 07974
S. A. Nikishin
Affiliation:
Nano Tech Center, Texas Tech University, Lubbock, Texas 79409Department of Electrical Engineering, Texas Tech University, Lubbock, Texas 79409
H. Temkin
Affiliation:
Nano Tech Center, Texas Tech University, Lubbock, Texas 79409Department of Electrical Engineering, Texas Tech University, Lubbock, Texas 79409
Get access

Abstract

We present results on growth and fabrication experiments of AlN/AlGaN superlattices for ultraviolet (UV) optoelectronic devices. Superlattices with extremely short periods have been studied. The AlN “barrier” layers are 0.5 nm thick, and the AlxGa1-xN “wells” are 1.25 nm thick, with x ∼ 0.08. This combination gives an average AlN mole fraction of 0.63 across one full period. The superlattice periods, AlN mole fractions, and energy gaps are determined using TEM, X-ray diffraction, and optical reflectance. They are all consistent with each other. For device fabrication, p-i-n structures are grown doped with Si (n-type) and Mg (p-type). The acceptor activation energy of ∼ 0.2 eV is found. Mesa structures are plasma etched using chlorine chemistry. Etch rates of AlN are ∼ 1/3 those of GaN under identical circumstances. Etch rates of 250 nm/min are used for the device structures. A light emitting diode, with primary emission at 280 nm is reported, and a detector with sensitivity edge at 260 nm are reported.