Hostname: page-component-7b7567c8c-48dgx Total loading time: 0 Render date: 2026-11-18T06:30:59.350Z Has data issue: false hasContentIssue false

Processing and Properties of Silver-Clad Tl-Ba-Ca-Cu-O Wires and Tapes

Published online by Cambridge University Press:  26 February 2011

K. C. Goretta
Affiliation:
Argonne National Laboratory, Argonne, IL 60439–4838
C. -T. Wu
Affiliation:
Argonne National Laboratory, Argonne, IL 60439–4838
M. T. Lanagan
Affiliation:
Argonne National Laboratory, Argonne, IL 60439–4838
M. A. Boling
Affiliation:
Argonne National Laboratory, Argonne, IL 60439–4838
Donglu Shi
Affiliation:
Argonne National Laboratory, Argonne, IL 60439–4838
D. J. Miller
Affiliation:
Argonne National Laboratory, Argonne, IL 60439–4838
Nan Chen
Affiliation:
Argonne National Laboratory, Argonne, IL 60439–4838
W. G. Hanewald
Affiliation:
Argonne National Laboratory, Argonne, IL 60439–4838
S. Sengupta
Affiliation:
Argonne National Laboratory, Argonne, IL 60439–4838
Z. Wang
Affiliation:
Argonne National Laboratory, Argonne, IL 60439–4838
R. B. Poeppel
Affiliation:
Argonne National Laboratory, Argonne, IL 60439–4838
F. Foong
Affiliation:
University of Nebraska, Lincoln, NE 68588–0111
S. H. Liou
Affiliation:
University of Nebraska, Lincoln, NE 68588–0111
Get access

Abstract

TlBA2Cu3Ox and Tl2Ca2Cu3Ox powders were synthesized, loaded into Ag tubes, and worked into wires and tapes by drawing and rolling. All processing outside of furnaces was in a dry-N2 glovebox. All heat treatments were performed in O2. The Ag-clad wires fabricated from these powders exhibited onset of superconductivity at ≈118 K and critical current densities at 77 K of 2 × 103 to 4 ×103 A/cm2.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable