Hostname: page-component-7b7567c8c-slfcl Total loading time: 0 Render date: 2026-11-19T15:35:56.495Z Has data issue: false hasContentIssue false

The Quaternary System Fe-Cr-Mn-C and Aligned Ferrous Superalloys

Published online by Cambridge University Press:  15 February 2011

F. D. Lemkey
Affiliation:
United Technologies Research Center, East Hartford, CT 06108
E. R. Thompson
Affiliation:
United Technologies Research Center, East Hartford, CT 06108
J. C. Schuster
Affiliation:
Institute of Physical Chemistry,University of Vienna, Austria
H. Nowotny
Affiliation:
University of Connecticut, Storrs, CT 06268
Get access

Abstract

A challenge exists for wider application of low cost iron-base alloys in the extreme conditions of high temperature, hot corrosion, and high stress experienced in gas turbine engines. In response to this challenge the constitution of the quaternary, Fe-Cr-Mn-C, and to a lesser extent the quinary, Fe-Cr-Mn-Al-C, systems were examined for in situ composite alloy candidates. Multivariant eutectic compositions, determined from phase equilibria, were directionally solidified to produce aligned composites consisting of M7C3 carbides within a gamma iron matrix. The composition and lattice parameters of the carbide and matrix phases were determined to establish their respective stabilities. Stress rupture tests in the direction of phase alignment for certain compositions (e.g., Fe-20 wt% Cr-lO wt% Mn-3.2 wt% C) indicated strength values comparable to cast nickel-base superalloys and exceeded those of the strongest iron-nickel superalloys developed for automotive turbines. Results of cyclic sulfidation testing at 9000 indicated a balance of Cr and Al content to be important to the achievement of outstanding surface stability.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1982

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable