Hostname: page-component-7b7567c8c-fvjsw Total loading time: 0 Render date: 2026-11-16T21:21:26.419Z Has data issue: false hasContentIssue false

Solid-Phase Reaction of Tungsten Thin Films with Polycrystalline Diamond

Published online by Cambridge University Press:  21 February 2011

A. Bachli
Affiliation:
California Institute of Technology, Pasadena, CA 91125
J. S. Chen
Affiliation:
California Institute of Technology, Pasadena, CA 91125
R. P. Ruiz
Affiliation:
Jet Propulsion Laboratory, California Institute of Technology, CA 91109
M-A. Nicolet
Affiliation:
California Institute of Technology, Pasadena, CA 91125
Get access

Abstract

The thermally induced solid-phase reaction of 135 nm thick sputter-deposited W films with polycrystalline CVD-grown diamond substrates is investigated. The samples are annealed in vacuum (5×10/-7 torr) at temperatures between 700 °C and 1100 °C for 1 hour and examined by 2 MeV 4He++ backscattering spectrometry, x-ray diffraction, and scanning electron microscopy.

The as-deposited W films contain roughly 5 at.% oxygen. After annealing the samples at 800 °C this oxygen concentration falls below the detection limit of less than 1 %. Incipient W2C phase formation occurs during annealing at 900 °C. The final state, the WC phase, is reached after annealing at 1100 °C.