Hostname: page-component-7b7567c8c-z4zkx Total loading time: 0 Render date: 2026-11-16T14:51:58.922Z Has data issue: false hasContentIssue false

Superplasticity of Liquid-Phase Sintered β-SiC

Published online by Cambridge University Press:  10 February 2011

T. Nagano
Affiliation:
Ceramics Superplasticity Project, ICORP, Japan Science and Technology Corporation, 2-4-1, Mutsuno, Atsuta-ku, Nagoya 456-8587, Japan nagano@ngo.jst.go.jp
K. Kaneko
Affiliation:
Ceramics Superplasticity Project, ICORP, Japan Science and Technology Corporation, 2-4-1, Mutsuno, Atsuta-ku, Nagoya 456-8587, Japan nagano@ngo.jst.go.jp
G.D. Zhan
Affiliation:
National Institute for Research in Inorganic Materials, 1-1, Namiki, Tsukuba 305-0044, Japan
M. Mitomo
Affiliation:
National Institute for Research in Inorganic Materials, 1-1, Namiki, Tsukuba 305-0044, Japan
Get access

Abstrtact

The compression and the tension tests of liquid-phase sintered β-SiC fabricated by hot-pressing using ultra fine powders were performed at 1973 K ∼ 2048 K in N2 atmosphere. Amorphous phases were observed at the grain boundaries and at multi-grain junctions in the assintered material. Strain hardening was observed under all experimental conditions. Stress exponents in the compression test were from 1.7 to 2.1 in the temperature ranging from 1973 K to 2023 K. A maximum tensile elongation of 170 % was achieved at the initial strain rate of 2 Χ 10−5 s−1 at 2048 K.