Hostname: page-component-7b7567c8c-z4zkx Total loading time: 0 Render date: 2026-11-17T10:54:24.150Z Has data issue: false hasContentIssue false

Ta-Si-N and Si3N4 Encapsulants for InP

Published online by Cambridge University Press:  25 February 2011

J. S. Reid
Affiliation:
California Institute of Technology, Pasadena, CA 91125
R. P. Ruiz
Affiliation:
Jet Propulsion Laboratory, Pasadena, CA 91109
E. Kolawa
Affiliation:
California Institute of Technology, Pasadena, CA 91125
J. S. Chen
Affiliation:
California Institute of Technology, Pasadena, CA 91125
J. Madok
Affiliation:
University of California, Los Angeles, CA 90024
M -A. Nicolet
Affiliation:
California Institute of Technology, Pasadena, CA 91125
Get access

Abstract

Thin films of sputtered, amorphous Ta36Si14N50 (a metallic conductor) and Si3N4 (an insulator) were evaluated as encapsulants for (100)-oriented InP substrates. Thicknesses of both films were approximately 100 nm. During a 15 min annealing in Ar, liberated phosphorus was gettered by a <Si>ISiO2ITa(100 nm) collector placed face-to-face on encapsulated or non-encapsulated InP. The stability of the InP with the encapsulant was characterized by backscattering spectrometry, scanning electron microscopy, and x-ray diffraction. As measured by 4He++ backscattering spectrometry, detectable amounts of phosphorus do not arise in the Ta collectors for the Ta-Si-N and Si3N4 encapsulation schemes until 650 and 700°C, respectively. Failure of the Ta36Si14N50 film is catastrophic at 700°C whereas the Si3N4 film degrades locally commencing at 600°C.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable