Hostname: page-component-7b7567c8c-fvjsw Total loading time: 0 Render date: 2026-11-17T10:13:16.361Z Has data issue: false hasContentIssue false

D-57 Lattice Strain Development and Strain-Induced Phase Transformation During Fatigue of a Cobalt-Based Superalloy

Published online by Cambridge University Press:  20 May 2016

M. L. Benson
Affiliation:
The University of Tennessee, Knoxville, TN
T. A. Saleh
Affiliation:
The University of Tennessee, Knoxville, TN
P. K. Liaw
Affiliation:
The University of Tennessee, Knoxville, TN
H. Choo
Affiliation:
The University of Tennessee, Knoxville, TN
R. A. Buchanan
Affiliation:
The University of Tennessee, Knoxville, TN
X.-L. Wang
Affiliation:
Oak Ridge National Laboratory, Oak Ridge, TN
A. D. Stoica
Affiliation:
Oak Ridge National Laboratory, Oak Ridge, TN
M. R. Daymond
Affiliation:
Rutherford Appleton Laboratory, OX, UK
D. W. Brown
Affiliation:
Los Alamos National Laboratory, Los Alamos, NM
D. L. Klarstrom
Affiliation:
Haynes International, Inc., Kokomo, IN
Get access

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'

Information

Type
Denver X-Ray Conference
Copyright
Copyright © Cambridge University Press 2004

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable