No CrossRef data available.
Published online by Cambridge University Press: 29 February 2012
Crystal structure of 4H-SiC was refined from room-temperature X-ray powder diffraction data using the Rietveld refinement method. The refined lattice constants were determined to be a=b=3.079 93(0) Å, c=10.082 22(2) Å, and the refined overall temperature factor B=0.383(3) Å2. Using the Debye approximation, the Debye temperature was successfully determined to be 1194.8 K.