Effects of hydrogen on the interactions of fuel cell sealing glasses with interconnect alloys

Published online by Cambridge University Press:  29 February 2012

S. T. Misture*
Affiliation:
New York State College of Ceramics at Alfred University, Alfred, New York 14802
*
a)Electronic mail: misture@alfred.edu
Get access

Abstract

In situ X-ray diffraction was used to study the interactions of the PNNL G18 fuel cell sealing glasses with the oxides that form on candidate interconnect alloys and with the ebrite alloy. Experiments under 4% hydrogen and air at temperatures up to 1000 °C showed that the sealant reacts rapidly with alumina and chromia, but not with NiO. The crystallization of the high-CTE phase BaCrO4 was noted for G18 in contact with chromia or ebrite under air, but reducing conditions inhibit the crystallization. The reactions in all cases begin within a few hours at temperatures above 800 °C and go to completion or near completion after ∼12 h.

Information

Type
X-Ray Diffraction
Copyright
Copyright © Cambridge University Press 2008

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable