Equal channel angular pressing processing routes and associated structure modification: a differential scanning calorimetry and X-ray line profile analysis

Published online by Cambridge University Press:  17 August 2012

A. Sarkar*
Affiliation:
Department of Materials Engineering, Indian Institute of Science, Bangalore 560012, India
Satyam Suwas
Affiliation:
Department of Materials Engineering, Indian Institute of Science, Bangalore 560012, India
D. Goran
Affiliation:
LEM3, Université Paul Verlaine de Metz, Ile du Saulcy, 57045 Metz Cedex 1, France
J.-J. Fundenberger
Affiliation:
LEM3, Université Paul Verlaine de Metz, Ile du Saulcy, 57045 Metz Cedex 1, France
L.S. Toth
Affiliation:
LEM3, Université Paul Verlaine de Metz, Ile du Saulcy, 57045 Metz Cedex 1, France
T. Grosdidier
Affiliation:
LEM3, Université Paul Verlaine de Metz, Ile du Saulcy, 57045 Metz Cedex 1, France
*
a)Author to whom correspondence should be addressed. Electronic mail: apusarkar@gmail.com

Abstract

The effectiveness of different routes of equal channel angular pressing (A, Bc, and C) is studied for commercially pure copper. The stored energy and the activation energy of recrystallization for the deformed samples were quantified using differential scanning calorimetry and X-ray diffraction line profile analysis. Results of the study revealed that the dislocation density and the stored energy are higher in the case of route Bc deformed sample. The activation energy for recrystallization is lower for route Bc.

Information

Type
Technical Articles
Copyright
Copyright © International Centre for Diffraction Data 2012
Figure 0

Figure 1. (Color online) DSC thermograms for Cu samples deformed up to four ECAP passes using different routes.

Figure 1

Figure 2. (Color online) Plot for Kissinger analysis to determine activation energy for Cu sample after four ECAP passes using different routes.

Figure 2

TABLE I. Results obtained from DSC study of four pass deformed samples.

Figure 3

Figure 3. X-ray diffraction profiles for Cu sample after four ECAP passes using different routes.

Figure 4

Figure 4. (Color online) Whole pattern fit of the XRD profile for Cu sample after four ECAP passes using route C.

Figure 5

Figure 5. (Color online) Classical Williamson–Hall plot for Cu samples after four ECAP passes using different routes.

Figure 6

Figure 6. MWP fit of XRD intensity profile for Cu sample after four ECAP passes using route C.

Figure 7

TABLE II. Results of MWP fit of the XRD profiles of samples deformed up to four passes using different routes.

Figure 8

Figure 7. (Color online) Crystallite size distribution function for Cu samples after four ECAP passes using different routes.