S15 Micro Stress Accumulation in Multiphase Superalloys

Published online by Cambridge University Press:  20 May 2016

J. Repper
Affiliation:
TU München, Garching, Germany
M. Hofmann
Affiliation:
TU München, Garching, Germany
W. Petry
Affiliation:
TU München, Garching, Germany
C. Krempaszky
Affiliation:
TU München, Garching, Germany
E. Werner
Affiliation:
TU München, Garching, Germany
Get access

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'

Information

Type
DENVER X-RAY CONFERENCE
Copyright
Copyright © Cambridge University Press 2008

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable