Hostname: page-component-7b7567c8c-tnkh4 Total loading time: 0 Render date: 2026-11-18T02:11:43.683Z Has data issue: false hasContentIssue false

The Effect of Nitrogen Ion Damage on the Optical and Electrical Properties of MBE GaN Grown on MOCVD GaN/sapphire Templates

Published online by Cambridge University Press:  13 June 2014

Alexander P Young
Affiliation:
Department of Electrical Engineering, The Ohio-State University, 2015 Neil Avenue, Columbus, OH 43210-1272, U.S.A.
Leonard J. Brillson
Affiliation:
Department of Electrical Engineering, The Ohio-State University, 2015 Neil Avenue, Columbus, OH 43210-1272, U.S.A.
Yoshiki Naoi
Affiliation:
Department of Electrical Engineering, University of California, San Diego, 9500 Gilman Dr., La Jolla, CA 92093-0407, U.S.A.
Charles W. Tu
Affiliation:
Department of Electrical Engineering, University of California, San Diego, 9500 Gilman Dr., La Jolla, CA 92093-0407, U.S.A.

Abstract

We have established a correlation between localized states responsible for mid-gap optical emission and film mobility of GaN grown under different nitrogen conditions. By imposing a deflector voltage at the tip of the plasma source, we varied the ion/neutral flux ratio to determine how N ions affect mid-gap luminescence and electrical mobility. Low energy electron-excited nanometer scale luminescence (LEEN) spectroscopy in ultrahigh vacuum (UHV) showed mid-gap emission intensities in the bulk that decreased in the ratio, 50 : 1.3 : 1 with increasing deflector voltage. Hall measurements indicated over a factor of two increase in mobility, and a factor of 8 decrease in residual charge density with increasing deflector voltage. The correlation of optical and electrical properties with a reduction in N ion flux suggests the primary role of native defects, such as N or Ga vacancies, in the mid-gap emissions.

Information

Type
Research Article
Copyright
Copyright © 1996 Materials Research Society
Figure 0

Table I.Electrical properties of GaN grown with successively greater plate deflection voltage. As the plate voltage is applied, the mobility increases, and correspondingly, the residual charge density decreases. All Measurements were made at 300K.

Figure 1

Figure 1.LEEN luminescence intensity as a function of electron beam penetration depth for GaN grown with plate voltage = 700 V. The right side of the figure indicates the beam voltage and the corresponding electron beam penetration depth in nm.

Figure 2

Figure 2.Close up of the band edge showing the reduction of the D-A peak as a function of plate voltage applied to the N beam flux during GaN growth. Spectra are offset for clarity.

Figure 3

Figure 3.Comparison of LEEN spectra for GaN grown as a function of plate voltage. At an electron beam energy of 3.0 keV, the beam penetrates to a maximum depth of 140 nm, comparable to the penetration depth of a He-Cd laser.